Price Exc Tax
1Kg-3kg packs.
Ferritic/Martensitic stainless has chromium levels of 12% - 18% as the main alloying element and has carbon levels toenable air hardening to a predominantly martensitic structure. Accordingly, detailed attention must be paid to both pre-heatand PWHT during and after welding.
Standard austenitic are those in the ASTM 3XX series and should, in the main, be welded with matching electrodes and for all fabrication, purposes should be considered non-hardenable, non-heat-treatable and thus show no PWHT requirement.
AWS A5.4 E316L-17
Diameter | Current (A) |
---|---|
1.6mm | 20-40 |
2.4mm | 40-60 |
3.2mm | 75-120 |
4.0mm | 100-160 |